Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 49.0 MPa @Temperature 1095 °C |
7110 psi @Temperature 2003 °F |
|
Pyrotek Pyrocast PCR Abrasion-Resistant Refractory Castable Pyrocast PCR is an abrasion resistant, thermal shock resistant castable. It is suitable to give exceptional resistance for conditions such as rapid heating or rapid cooling.ApplicationsCarbon anode.. |
|||
Compressive Strength | 49.0 MPa @Strain 2 % |
7110 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Compressive Strength | >= 49.0 MPa @Temperature 1100 °C |
>= 7110 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics PHOSTCAST 60 XL Phosphate Bonded Castables Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and .. |
|||
Compressive Strength | 49.0 MPa @Temperature 1500 °C |
7110 psi @Temperature 2730 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST 80 High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 49.0 MPa @Temperature 1500 °C |
7110 psi @Temperature 2730 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST C SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 49.0 MPa @Temperature 110 °C |
7110 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 49.0 MPa @Temperature 110 °C |
7110 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST SPECIAL Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | 49.0 MPa @Temperature 1400 °C |
7110 psi @Temperature 2550 °F |
Cold Crushing |
Sharadaa Ceramics Sharada RFC-45 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 49.0 MPa @Temperature 800 °C |
7110 psi @Temperature 1470 °F |
Cold Crushing |
Sharadaa Ceramics Sharada RFC-80 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 49.0 MPa @Temperature 1400 °C |
7110 psi @Temperature 2550 °F |
Cold Crushing |
Sharadaa Ceramics Sharada RFC-Fused Silica Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 49.0 MPa @Temperature 1500 °C |
7110 psi @Temperature 2730 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST C High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 49.0 MPa @Temperature 1000 °C, Time 10800 sec |
7110 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories BPCT-170 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa @Temperature 1500 °C, Time 10800 sec |
7110 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CTC-63TD Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 - 58.8 MPa @Temperature 1500 °C, Time 10800 sec |
7110 - 8530 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HAPT-80S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa @Temperature 1500 °C, Time 10800 sec |
7110 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories joint-1 Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa @Temperature 110 °C, Time 86400 sec |
7110 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories LPCT-17PI Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa @Temperature 110 °C, Time 86400 sec |
7110 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories SFC-60 SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa @Temperature 1350 °C, Time 10800 sec |
7110 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TCH-175S Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa @Temperature 1350 °C, Time 10800 sec |
7110 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TCH-175Y Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa @Temperature 1371 °C |
7110 psi @Temperature 2500 °F |
Cold Crush Strength |
BNZ Materials Blazecrete 3000 Dense Castable Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec.. |
|||
Compressive Strength | 49.0 MPa @Strain 2 % |
7110 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data) Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte.. |