Chosun Refractories SFC-60 SiC Castable

Category Ceramic , Carbide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SFC-60 SiC Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.008829 GPa

@Temperature 110 °C,
Time 86400 sec
1.281 ksi

@Temperature 230 °F,
Time 24.0 hour
0.017658 GPa

@Temperature 1000 °C,
Time 10800 sec
2.5611 ksi

@Temperature 1830 °F,
Time 3.00 hour
0.022563 GPa

@Temperature 1350 °C,
Time 10800 sec
3.2725 ksi

@Temperature 2460 °F,
Time 3.00 hour
Compressive Strength 49.0 MPa

@Temperature 110 °C,
Time 86400 sec
7110 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
83.4 MPa

@Temperature 1000 °C,
Time 10800 sec
12100 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
108 MPa

@Temperature 1350 °C,
Time 10800 sec
15600 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1600 °C
2910 °F
limited
Shrinkage -0.130 %

@Temperature 1350 °C,
Time 10800 sec
-0.130 %

@Temperature 2460 °F,
Time 3.00 hour
-0.0900 %

@Temperature 1000 °C,
Time 10800 sec
-0.0900 %

@Temperature 1830 °F,
Time 3.00 hour
-0.0300 %

@Temperature 110 °C,
Time 86400 sec
-0.0300 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 22 %
22 %
SiC 63 %
63 %
Descriptive Properties Value Comments
Installation Method Self Flowing
Material Required for Estimating(kg/?) 2,570