Chosun Refractories BPCT-170 Special Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories BPCT-170 Special Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Compressive Strength 49.0 MPa

@Temperature 1000 °C,
Time 10800 sec
7110 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
58.8 MPa

@Temperature 110 °C,
Time 86400 sec
8530 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage -0.0600 %

@Temperature 110 °C,
Time 86400 sec
-0.0600 %

@Temperature 230 °F,
Time 24.0 hour
0.22 %

@Temperature 1500 °C,
Time 10800 sec
0.22 %

@Temperature 2730 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 65 %
65 %
SiO2 30 %
30 %
Descriptive Properties Value Comments
Installation Method Casting