Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories PTC-165 Plastic Refractory

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories PTC-165 Plastic Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 7.70e-7 - 0.00490 GPa

@Temperature 110 °C,
Time 86400 sec
0.000112 - 0.711 ksi

@Temperature 230 °F,
Time 24.0 hour
0.00981 - 0.012753 GPa

@Temperature 1350 °C,
Time 10800 sec
1.42 - 1.8497 ksi

@Temperature 2460 °F,
Time 3.00 hour
Compressive Strength 9.81 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
1420 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
24.5 - 34.3 MPa

@Temperature 1350 °C,
Time 10800 sec
3560 - 4980 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.5237 W/m-K

@Temperature 500 °C
10.558 BTU-in/hr-ft²-°F

@Temperature 932 °F
1.6400 W/m-K

@Temperature 1000 °C
11.363 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
limited
Shrinkage -0.950 %

@Temperature 1350 °C,
Time 10800 sec
-0.950 %

@Temperature 2460 °F,
Time 3.00 hour
-0.500 %

@Temperature 110 °C,
Time 86400 sec
-0.500 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Cr2O3 28 - 33 %
28 - 33 %
Descriptive Properties Value Comments
Main Applications Reaction resistance of slag Soaking pit Reheating furnace
Material Required for Estimating (kg/?) 3,200