Material Notes:
Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and grease pens.The #500 high-stability acrylic adhesive provides excellent adhesion to a variety of surfaces including stainless steel, polycarbonate, and polypropylene.55# densified kraft liner assures consistent die cutting.3M™ Label Material 7884 is UL recognized (File MH11410).Applications:Labeling of small or irregular shape containersLabels requiring long term bond and piece removalLabels requiring variable informationBarcode labels and rating platesProperty identification and asset labelingWarning, instructions, and service labels for durable goodsNameplates for durable goodsInformation provided by 3M
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Adhesive
81.3 microns
3.20 mil
Liner
94.0 microns
3.70 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.09861 kN/m
0.5625 pli
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.110 kN/m
0.625 pli
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.110 kN/m
0.625 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.1205 kN/m
0.6875 pli
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.131 kN/m
0.750 pli
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.131 kN/m
0.750 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.1424 kN/m
0.8125 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.1424 kN/m
0.8125 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.153 kN/m
0.875 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.153 kN/m
0.875 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.1643 kN/m
0.9375 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.18626 kN/m
1.0625 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.18626 kN/m
1.0625 pli
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.18626 kN/m
1.0625 pli
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.1972 kN/m
1.125 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.1972 kN/m
1.125 pli
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.20817 kN/m
1.1875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.23008 kN/m
1.3125 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.25199 kN/m
1.4375 pli
Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.263 kN/m
1.50 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.263 kN/m
1.50 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.2849 kN/m
1.625 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.2849 kN/m
1.625 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.29582 kN/m
1.6875 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.31773 kN/m
1.8125 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.31773 kN/m
1.8125 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.33964 kN/m
1.9375 pli
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.33964 kN/m
1.9375 pli
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.351 kN/m
2.00 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.40538 kN/m
2.3125 pli
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.4163 kN/m
2.375 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.42729 kN/m
2.4375 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.44921 kN/m
2.5625 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.44921 kN/m
2.5625 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.47112 kN/m
2.6875 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.5040 kN/m
2.875 pli
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.5040 kN/m
2.875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.51494 kN/m
2.9375 pli
Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.570 kN/m
3.25 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.570 kN/m
3.25 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.6355 kN/m
3.625 pli
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.64642 kN/m
3.6875 pli
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.657 kN/m
3.75 pli
Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.745 kN/m
4.25 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.789 kN/m
4.50 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.8108 kN/m
4.625 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type #500 High-stability acrylic
Liner 55# Densified kraft