Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 1% Secant Modulus, MD = 27000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil LD 051.LJ Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil LD 051.LT Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D638
LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent ..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D638
LyondellBasell Petrothene® GA501021 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent ..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D638
LyondellBasell Petrothene® GA501022 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent ..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D638
LyondellBasell Petrothene® GA501023 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent ..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
Westlake EF796 Low Density Polyethylene
Westlake Polyethylene EF796 is a low density formulation suggested for film applications requiring a good balance of properties such as converter film for industrial packaging and general-purpose pa..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
Westlake EF923 Low Density Polyethylene
Westlake Polyethylene EF923 is a low density formulation suggested for film applications that require a good balance of properties such as converter film for industrial packaging and general purpose..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
Westlake EN923 Low Density Polyethylene
Westlake Polyethylene EN923 is a low density formulation suggested for film applications where enhanced processability and high clarity are required. It is characterized by good tear strength, impa..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
Westlake EP310 Low Density Polyethylene
WESTLAKE polyethylene EP310 is a low-density polyethylene suggested for cast film bakery applications. This material has outstanding optical and processing properties.Application/UsesBakery bagsSoft..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
Westlake EP413 Low Density Polyethylene
WESTLAKE polyethylene EP413 is a low-density polyethylene recommended for blown or cast film clarity applications. This material has very good optical properties, and is suggested for bakery films ,..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
Westlake Hifor Xtreme SC74844 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74844 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip, high antiblock and processing aid. Films produce..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
Westlake Hifor Xtreme SC74853 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74853 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and processing aid. Films produced wi..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
Westlake Hifor Xtreme SC74858 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74858 polymer is a high strength, good clarity linear low density polyethylene designed for blown film extrusion that contains no slip or antiblock and processing aid. Films ..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
Westlake LF1020 Butene Linear Low Density Polyethylene
Westlake LF1020 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant ..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade)
Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil Exceed™ 1018KB Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018KB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018KB resin have outstanding tensile, impact strength and puncture. These superior strength ..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin (Asia Pacific Grade)
Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil Exceed™ 1018MK Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil LD 051.LQ Shrink Film Resin
L Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding pr..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil LDPE LD 051.LQ Low Density Polyethylene Resin
Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding proc..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil Exceed™ 1018JA Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin
Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The..
Copyright © lookpolymers.com All Rights Reserved