Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil LD 051.LJ Shrink Film Resin
(discontinued **) LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil LD 051.LT Shrink Film Resin
(discontinued **) LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D638 |
LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D638 |
LyondellBasell Petrothene® GA501021 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D638 |
LyondellBasell Petrothene® GA501022 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D638 |
LyondellBasell Petrothene® GA501023 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
Westlake EF796 Low Density Polyethylene Westlake Polyethylene EF796 is a low density formulation suggested for film applications requiring a good balance of properties such as converter film for industrial packaging and general-purpose pa.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
Westlake EF923 Low Density Polyethylene Westlake Polyethylene EF923 is a low density formulation suggested for film applications that require a good balance of properties such as converter film for industrial packaging and general purpose.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
Westlake EN923 Low Density Polyethylene Westlake Polyethylene EN923 is a low density formulation suggested for film applications where enhanced processability and high clarity are required. It is characterized by good tear strength, impa.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
Westlake EP310 Low Density Polyethylene WESTLAKE polyethylene EP310 is a low-density polyethylene suggested for cast film bakery applications. This material has outstanding optical and processing properties.Application/UsesBakery bagsSoft.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
Westlake EP413 Low Density Polyethylene WESTLAKE polyethylene EP413 is a low-density polyethylene recommended for blown or cast film clarity applications. This material has very good optical properties, and is suggested for bakery films ,.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
Westlake Hifor Xtreme SC74844 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74844 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip, high antiblock and processing aid. Films produce.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
Westlake Hifor Xtreme SC74853 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74853 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and processing aid. Films produced wi.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
Westlake Hifor Xtreme SC74858 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74858 polymer is a high strength, good clarity linear low density polyethylene designed for blown film extrusion that contains no slip or antiblock and processing aid. Films .. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
Westlake LF1020 Butene Linear Low Density Polyethylene Westlake LF1020 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant .. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018KB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018KB resin have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018MK Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil LD 051.LQ Shrink Film Resin L Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding pr.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil LDPE LD 051.LQ Low Density Polyethylene Resin Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding proc.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018JA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
1% Secant Modulus, MD | 186 MPa | 27000 psi | ASTM D882 |
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The.. |