Material Notes:
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength properties, along with excellent drawability, makes this a very versatile packaging film. Availability: Latin America, North America and South AmericaAdditive:Antiblock: NoSlip: NoProcessing Aid: YesThermal Stabilizer: YesApplications:Agricultural FilmBag in BoxBarrier Food PackagingBlown FilmBlown Stretch FilmBread BagsFood packagingForm Fill and Seal PackagingFreezer FilmGeneral PackagingHeavy Duty Bags Lamination FilmMultilayer Packaging FilmOverwrap FilmPackaging FilmsPremium Trash Bags Stand Up PouchesTrash Bags Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ExxonMobil method
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
Film Elongation at Break, MD 480 %
480 %
ASTM D882
Film Elongation at Break, TD 640 %
640 %
ASTM D882
Puncture Energy 3.95 J
2.92 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 250 g
250 g
ASTM D1922
Elmendorf Tear Strength TD 430 g
430 g
ASTM D1922
Dart Drop Test 590 g
1.30 lb
ASTM D1709
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
Film Tensile Strength at Break, TD 53.1 MPa
7700 psi
ASTM D882
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 245 °C
<= 473 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 29 %
29 %
ASTM D1003
Gloss 28 %
28 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 11 lbf
ExxonMobil Method