Westlake EN923 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Westlake Chemical Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EN923 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake Polyethylene EN923 is a low density formulation suggested for film applications where enhanced processability and high clarity are required. It is characterized by good tear strength, impact strength, a wide heat-sealing range and printability.Application/UsesFood packagingHousehold bagsHousehold wrapsFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 38.1 microns
1.50 mil
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 250 %
250 %
ASTM D882
Film Elongation at Break, TD 750 %
750 %
ASTM D882
Dart Drop 2.63 g/micron
66.7 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
1% Secant Modulus, TD 221 MPa
32000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 4.5 %
4.5 %
ASTM D1003
Gloss 75 %
75 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 380 °F
with BUR of 2.4:1 or higher
Blow-up Ratio (BUR) 2.4
2.4
Descriptive Properties Value Comments
Process Film