Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 41.0 MPa | 5950 psi | ASTM D790 |
RedEye On Demand ABS for Rapid Prototyping ABS or Acrylonitrile butadiene styrene is a true industrial thermoplastic that is impact-resistant and structurally strong. ABS parts are built with a layered manufacturing process utilizing Fused D.. |
|||
Flexural Yield Strength | 41.0 - 75.8 MPa | 5950 - 11000 psi | Average value: 64.8 MPa Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Flexural Yield Strength | 41.0 MPa | 5950 psi | ASTM D790 |
PolyOne Lubri-Tech™ AS-000/10T-2S ABS - 10% PTFE - 2% Silicone
(discontinued **) Data provided by PolyOne. |
|||
Flexural Yield Strength | 41.0 MPa | 5950 psi | at 3.5% strain; 6% strain at break; ISO 178 |
FKuR Kunststoff Fibrolon® P 8540 Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Fibrolon® P 8540 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C.. |
|||
Flexural Yield Strength | 41.0 MPa | 5950 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Flexural Yield Strength | 41.0 MPa | 5950 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Flexural Yield Strength | 41.0 MPa | 5950 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON CX99000 PS (Europe-Africa-Middle East) LNP* STAT-KON* CX99000 is a compound based on Polystyrene containing Carbon Powder. Added features include : Electrically Conductive, Easy Molding. |
|||
Flexural Yield Strength | 41.0 MPa | 5950 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MX01739C PP LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Flexural Yield Strength | 41.0 MPa | 5950 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Flexural Yield Strength | 41.0 MPa | 5950 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MK001AS PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MK001AS is a compound based on Polypropylene resin containing Mineral. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Flexural Yield Strength | 41.0 MPa | 5950 psi | ASTM D790 |
Tipco Tipcolene® FPW 35 - 35% Wollastonite Reinforced Polypropylene Homopolymer, High Heat Stability 35% Wollastonite Reinforced PP HomopolymerApplications: Automotive & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 41.0 MPa | 5950 psi | ASTM D790 |
Washington Penn PPH5CF5 Polypropylene, 50% Calcium Carbonate Filled UV Stabilized; Injection molding grade.Applications: Commonly used as a concentrate. High flow for thin wall parts requiring long-flow. Toys, small appliances, outdoor furniture.Data provided by W.. |
|||
Flexural Yield Strength | 41.0 MPa | 5950 psi | 2 mm/min; ISO 178 |
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |