Tipco Tipcolene® FPW 35 - 35% Wollastonite Reinforced Polypropylene Homopolymer, High Heat Stability

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® FPW 35 - 35% Wollastonite Reinforced Polypropylene Homopolymer, High Heat Stability.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
35% Wollastonite Reinforced PP HomopolymerApplications: Automotive & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break >= 10 %
>= 10 %
ASTM D638
Flexural Yield Strength 41.0 MPa
5950 psi
ASTM D790
Flexural Modulus 2.90 GPa
421 ksi
ASTM D790
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
ASTM D648