UV Stabilized; Injection molding grade.Applications: Commonly used as a concentrate. High flow for thin wall parts requiring long-flow. Toys, small appliances, outdoor furniture.Data provided by Washington Penn Plastic Co., Inc.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Melt Flow 12 - 16 g/10 min
12 - 16 g/10 min
Cond L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Flexural Yield Strength 41.0 MPa
5950 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
Tangent; ASTM D790
Gardner Impact 14.5 J
10.7 ft-lb
ASTM D3029