Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Flexural Yield Strength | 123 - 139 MPa | 17800 - 20200 psi | Average value: 133 MPa Grade Count:3 |
Overview of materials for Phenolic, Graphite Cloth Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Graphite Cloth Composite". Each property range of values reported is minimum and maximum value.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | |
Phenolic 37%, Graphite fabric 63% Phenolic - "91LD". Graphite fabric - "WCB" |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | DIN 53455; ASTM D790 |
Kolon KOLEFIN® KO133GM40 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN333MS Low Friction Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | DIN 53452; ASTM D790 |
Kolon Kopa® KN133 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN331F General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM AUT230 PEI (Europe-Africa-Middle East) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem AUT230M PEI Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are .. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem XH6050F PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was .. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM AUT230 PEI Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM AUT230 PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL EXNL0143 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX1736 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | ASTM D790 |
PlastxWorld CEVIAN® S1220 PC/ABS alloy Glass fiber reinforced PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | ASTM D790 |
Toyobo Vylopet® EMC415 PET/PBT Blend Key Feature: HB UL-94 ClassApplications: accessory componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical properties, high di.. |
|||
Flexural Yield Strength | 123 MPa | 17900 psi | ASTM D790 |
Entec Hyril® SAN500 Styrene Acrylonitrile Available in North America Features: Copolymer Form: PelletsInformation provided by Entec |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | ASTM D790 |
Cheng Yu Plastic FR200N Flame Retardant Nylon 66 |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | ISO 178 |
Bulk Molding Compounds BMC 665 Mineral filled, 20% glass reinforced polyester molding compound Description: BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good.. |
|||
Flexural Yield Strength | 123 MPa | 17800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF WF003I PBT (Europe-Africa-Middle East) LNP* Thermotuf* WF003I BLACK is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Yield Strength | 123 MPa @Thickness 3.20 mm |
17800 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical |