Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon Kopa® KN133 Nylon 6 Resin

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Kolon
Trade Name Kopa®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon Kopa® KN133 Nylon 6 Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent chemical resistance, Wide usage temperature, Good impact absorbing characteristics. Information provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
DIN 53479; ASTM D792
Water Absorption 1.8 %
1.8 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
DIN 53505; ASTM D785
Tensile Strength, Ultimate 82.0 MPa
11900 psi
DIN 53455; ASTM D638
Elongation at Break 95 %
95 %
DIN 53455; ASTM D638
Flexural Yield Strength 123 MPa
17800 psi
DIN 53452; ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
DIN 53452; ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 220 °C
428 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 180 °C
356 °F
DIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
DIN 53461; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.4

@Frequency 1e+6 Hz
3.4

@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149/DIN 53481
Arc Resistance 120 sec
120 sec
ASTM D495