Polymer Property : Flexural Yield Strength = 139 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 123 - 139 MPa
17800 - 20200 psi
Average value: 133 MPa Grade Count:3
Overview of materials for Phenolic, Graphite Cloth Composite
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Graphite Cloth Composite". Each property range of values reported is minimum and maximum value..