Phenolic - "91LD". Graphite fabric - "WCB"
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 68.74 MPa
9970 psi
Flexural Yield Strength 123 MPa
17800 psi
Flexural Modulus 8.07 GPa
1170 ksi
Compressive Yield Strength 75.2 MPa
10900 psi
Compressive Modulus 12.1 GPa
1750 ksi