Plenco 5482 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 5482 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for electrical insulating applications.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Water Absorption 0.247 %
0.247 %
ASTM D570
Linear Mold Shrinkage 0.0061 cm/cm
0.0061 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 89
89
ASTM D785
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 0.41 %
0.41 %
ASTM D638
Tensile Modulus 8.70 GPa
1260 ksi
ASTM D638
Flexural Strength 86.0 MPa
12500 psi
ASTM D790
Flexural Modulus 8.00 GPa
1160 ksi
ASTM D790
Compressive Strength 215 MPa
31200 psi
ASTM D695
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.194 J/cm²
0.923 ft-lb/in²
ASTM D256
Impact 96
96
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 201 °C
394 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 186 °C
367 °F
ASTM D648
Oxygen Index 28.5 %
28.5 %
ASTM D2863
Shrinkage 0.25 %
0.25 %
72 hr, 120ºC; ASTM D1299