Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON PD000 PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON PD000 PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* STAT-KON* PD000 is a compound based on PA 6 resin containing Carbon Powder. Added features include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0138 cm/cm
0.0138 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 54.0 MPa
7830 psi
5 mm/min; ISO 527
Tensile Strength, Yield 55.0 MPa
7980 psi
5 mm/min; ISO 527
Elongation at Break 1.4 %
1.4 %
5 mm/min; ISO 527
6.9 %
6.9 %
Flexural Strain, break, 2 mm/min; ISO 178
Elongation at Yield 1.4 %
1.4 %
5 mm/min; ISO 527
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min; ISO 527
Flexural Strength 124 MPa
18000 psi
2 mm/min; ISO 178
Flexural Yield Strength 125 MPa
18100 psi
2 mm/min; ISO 178
Flexural Modulus 3.90 GPa
566 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
40.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Electrical Properties Metric English Comments
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D257