Material Notes:
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact compliantInformation provided by Victrex
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Crystalline; ISO 1183
Viscosity 200000 cP

@Temperature 400 °C
200000 cP

@Temperature 752 °F
Melt; ISO 11443
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ISO 527
Elongation at Break 10 %
10 %
ISO 527
Tensile Modulus 4.30 GPa
624 ksi
ISO 527
Flexural Strength 170 MPa
24700 psi
ISO 178
Flexural Modulus 4.00 GPa
580 ksi
ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/A
Izod Impact, Unnotched (ISO) NB
NB
ISO 180/U
Thermal Properties Metric English Comments
Melting Point 373 °C
703 °F
ISO 11357
Glass Transition Temp, Tg 152 °C
306 °F
Onset; ISO 11357
160 °C
320 °F
Midpoint; ISO 11357
Processing Properties Metric English Comments
Processing Temperature 400 - 420 °C
752 - 788 °F
Drying Temperature 120 °C

@Time 18000 sec
248 °F

@Time 5.00 hour
150 °C

@Time 10800 sec
302 °F

@Time 3.00 hour
Descriptive Properties Value Comments
Color Natural