Material Notes:
Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
NCMT Method
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 5.70 GPa
827 ksi
ASTM D638
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 170 °C
338 °F
Deflection Temp.; ASTM D648