LG Chemical Lupoy 1603-03 Polycarbonate Resin

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer LG Chemical
Trade Name LUPOY
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical Lupoy 1603-03 Polycarbonate Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: LUPOY PC 1603-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: UV Stabilizer, High viscosity, Good mold release and High melt strengthApplications: Structure sheets and Multi-wall sheetsCAS: 103598-77-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.32 %

@Temperature 23.0 °C
0.32 %

@Temperature 73.4 °F
equilibrium, 50% RH; ASTM D570
0.15 %

@Temperature 23.0 °C,
Time 86400 sec
0.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
3.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 72.0 MPa
10400 psi
ASTM D638
Tensile Strength, Yield 60.0 MPa
8700 psi
50mm/min; ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D638
Flexural Yield Strength 96.0 MPa
13900 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 9.608 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
18.00 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
Izod Impact, Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 146 °C

@Thickness 4.00 mm
295 °F

@Thickness 0.157 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C

@Thickness 4.00 mm
270 °F

@Thickness 0.157 in
Unannealed; ASTM D648
143 °C

@Thickness 4.00 mm
289 °F

@Thickness 0.157 in
Annealed; ASTM D648
Vicat Softening Point 151 °C

@Load 5.10 kg
304 °F

@Load 11.2 lb
50°C/hr; ASTM D1525
Softening Point 150 - 200 °C
302 - 392 °F
melting point per MSDS
Flash Point >= 450 °C
>= 842 °F
Optical Properties Metric English Comments
Refractive Index 1.586
1.586
ASTM D542
Haze 0.70 - 1.5 %
0.70 - 1.5 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003
Descriptive Properties Value Comments
Autoignition Temperature >450°C
Users viewing this material also viewed the following: