M. Holland Company GS230 Polystyrene, General Purpose

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Heat Resistant Grade
Manufacturer M. Holland Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company GS230 Polystyrene, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High heat resistanceGood processabilityHigh strengthApplications: BottlesBusiness equipmentMedical applicationsPackaging
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.3 MPa
7000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D638
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 93.9 °C
201 °F
Unannealed; ASTM D648
Vicat Softening Point 109 °C
228 °F
ASTM D1525
Descriptive Properties Value Comments
Forms Pellets
Processing Methods Extrusion, injection molding