Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styron CALIBREâ„¢ 302-6 Polycarbonate Resin

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Styron
Trade Name CALIBRE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron CALIBREâ„¢ 302-6 Polycarbonate Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: CALIBREâ„¢ 300-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, and optical clarity as well as high melt strength for blow molding and sheet applications. The CALIBRE 300-6 series products are available in 4 additive packages: CALIBRE 300: No mold release or UV Stabilizer. CALIBRE 301: Mold release. CALIBRE 302: UV stabilizer. CALIBRE 303: Mold release and UV stabilizerGovt. and Industry Standards: CSA (Canadian Standards Association)Underwriters Laboratory Inc. (UL) Applications:Automotive interiorsAutomotive exteriorsSheet applicationsElectrical lighting/switchesSmall & large appliancesBeverage containers/servicewarePowder equipmentInformation provided by Styron
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/A; ASTM D792
Water Absorption 0.25 %

@Temperature 23.0 °C
0.25 %

@Temperature 73.4 °F
Equilibrium, 50% RH; ISO 62; ASTM D570
0.15 %

@Temperature 23.0 °C,
Time 86400 sec
0.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ISO 294-4; ASTM D955
Melt Flow 6.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
6.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 73
73
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength at Break 72.0 MPa
10400 psi
ISO 527-2/50
72.4 MPa
10500 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa
8700 psi
50 mm/min; ISO 527-2/50; ASTM D638
Elongation at Break 150 %
150 %
50 mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
50 mm/min; ISO 527-2/50; ASTM D638
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-2/50
2.41 GPa
350 ksi
50 mm/min; ASTM D638
Flexural Strength 96.5 MPa
14000 psi
Method I (3 point load), 2.0 mm/min; ASTM D790
97.0 MPa
14100 psi
3-point; ISO 178
Flexural Modulus 2.40 GPa
348 ksi
3-point; ISO 178
2.41 GPa
350 ksi
Method I (3 point load), 2.0 mm/min; ASTM D790
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Notched (ISO) 93.0 kJ/m²

@Temperature 23.0 °C
44.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Izod Impact, Unnotched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256; ISO 180
Charpy Impact, Notched 5.50 J/cm²

@Temperature 23.0 °C
26.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Tensile Impact Strength 588 kJ/m²
280 ft-lb/in²
ASTM D1822
Dart Drop, Total Energy 90.4 J
66.7 ft-lb
3.39 m/sec; ASTM D3763
Abrasion 45
45
[%] Taber; ASTM D1044
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Hot Ball Pressure Test 125 °C
257 °F
IEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Annealed; ASTM D648
146 °C
295 °F
Annealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
259 °F
Unannealed; ISO 75-2/B
129 °C
264 °F
Unannealed; ASTM D648
142 °C
288 °F
Annealed; ASTM D648
143 °C
289 °F
Annealed; ISO 75-2/B
Vicat Softening Point 151 °C

@Load 5.10 kg
304 °F

@Load 11.2 lb
Rate A (50°C/h); ISO 306/B50; ASTM D1525
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0626 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Oxygen Index 26 %
26 %
ISO 4289-2
Optical Properties Metric English Comments
Refractive Index 1.586
1.586
ASTM D542; ISO 489
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 60.0 Hz
3.0

@Frequency 60.0 Hz
ASTM D150
3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
17.0 kV/mm
432 kV/in
IEC 60243-1
Dissipation Factor 0.0010

@Frequency 50.0 Hz
0.0010

@Frequency 50.0 Hz
ASTM D150
0.0020

@Frequency 1.00e+6 Hz
0.0020

@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index 250 V

@Thickness 2.00 mm
250 V

@Thickness 0.0787 in
Solution A; IEC 60112
Descriptive Properties Value Comments
Average Extent of Burring 3 cm
ASTM D635
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved