Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Nilit Polynil® P50 Standard Viscosity Nylon 66 Description: Standard viscosityApplication: CompoundingInformation provided by NILIT. |
|||
Tensile Modulus | 3.03 GPa | 439 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific) ASA+PC may contain up to 20% post-industrial recycle. Excellent flow, weatherability, toughness and high heat for exterior uses. |
|||
Tensile Modulus | 3.03 GPa @Temperature 23.0 °C |
439 ksi @Temperature 73.4 °F |
ASTM D638 |
PolyOne Geon™ CPVC MC250 Polyvinyl Chloride, Chlorinated (CPVC) The Geon MC250 CPVC is an injection molding fittings compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geo.. |
|||
Tensile Modulus | 3.03 GPa | 439 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings M1000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 3.03 GPa | 439 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings M1005 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Nilit Polynil® P50L Externally Lubricated Nylon 66 Description: Polynil P50L is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips. It is also suited for monofilament extrusion.Key characteristics: Ex.. |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Quadrant EPP Duratron® PAI T4501 Polyamide-imide, compression molded bearing grade (ASTM Product Data Sheet) |
|||
Tensile Modulus | 3.03 GPa | 439 ksi | ASTM D638 |
LNP Lubricomp® PDX-E-00548 CCS Polyetherimide, Aramid Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: Lubricated, Low to None Ion ContentForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however man.. |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Fiberfil® J-60/10/E Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Fiberfil® J-60/10/E8 Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 3.03 GPa | 439 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP EX00548C PEI LNP LUBRICOMP* EX00548C is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Clean Compounding System, Wear Resistant. |
|||
Tensile Modulus | 3.03 GPa | 439 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 3.03 GPa | 439 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel. |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Total PSC 523 Polystyrene Polystyrene 523 is a high flow, high heat crystal. Specially designed for foam applications it has a very narrow molecular weight distribution. Performance in extruded loose fill foam is excellent d.. |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Total PSC 524B Polystyrene Polystyrene 524B is a general purpose crystal polystyrene targeted for gloss coextrusion cap applications. It is specially formulated to reduce die buildup and die lines.Information provided by Tota.. |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Total PSC 525 Polystyrene Polystyrene 525 is a crystal polystyrene for both injection molding and cap layer co-extrusion. Injection molding applications such as medical and laboratory parts, tumblers and jewel boxes demonstr.. |
|||
Tensile Modulus | 3.03 GPa | 439 ksi | 90 Minute UV Cure; SLA 3500 System; ASTM D638 |
3D Systems Accura® accuGen™ Nd Plastic for SLA® Systems Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® Viper si2™, 3500, 5000 & 7000 systems.Typical ApplicationsMulti-purpose mode.. |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D-638 |
Axiall 7020 Rigid PVC, Extrusion Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityF.. |
|||
Tensile Modulus | 3.03 GPa | 439 ksi | ASTM Data |
Americas Styrenics Styron® 425 High Impact Polystyrene
(discontinued **) STYRON® 425 impact polystyrene resin is typically used in thin section parts, hot drink cups and cassettes. It offers heat resistance, easy flow, fast cycling, and excellent tensile and flex proper.. |