Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ CPVC MC250 Polyvinyl Chloride, Chlorinated (CPVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , Chlorinated PVC (CPVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ CPVC MC250 Polyvinyl Chloride, Chlorinated (CPVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Geon MC250 CPVC is an injection molding fittings compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geon MC250 demonstrates ease of processing and excellent thermal stability.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Yield 55.8 MPa

@Temperature 23.0 °C
8090 psi

@Temperature 73.4 °F
ASTM D638
Tensile Modulus 3.03 GPa

@Temperature 23.0 °C
439 ksi

@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength 108 MPa
15700 psi
ASTM D790
Flexural Modulus 3.50 GPa
508 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
217 °F
Annealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 198 - 210 °C
388 - 410 °F
Descriptive Properties Value Comments
Agency Ratings NSF 14
NSF 61
UL 94
Pass - Not Listed
Forms Pellets
Generic Material CPVC
Generic Name Polyvinyl Chloride, Chlorinated (CPVC)
Processing Method Injection Molding
PVC Cell Classification 23447
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Fittings
Industrial Applications
Users viewing this material also viewed the following: