Total PSC 524B Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer Total Atofina
Trade Name PSC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSC 524B Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polystyrene 524B is a general purpose crystal polystyrene targeted for gloss coextrusion cap applications. It is specially formulated to reduce die buildup and die lines.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.2 MPa
6700 psi
ASTM D638
Tensile Modulus 3.03 GPa
440 ksi
ASTM D638
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Flexural Modulus 3.03 GPa
440 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 96.7 °C
206 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 101 °C
213 °F
ASTM D1525