Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PSC 523 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer Total Atofina
Trade Name PSC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSC 523 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polystyrene 523 is a high flow, high heat crystal. Specially designed for foam applications it has a very narrow molecular weight distribution. Performance in extruded loose fill foam is excellent due to the tailored molecular weight profile.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 11 g/10 min

@Load 5.00 kg,
Temperature 200 °C
11 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Tensile Modulus 3.03 GPa
440 ksi
ASTM D638
Flexural Strength 82.0 MPa
11900 psi
ASTM D790
Flexural Modulus 3.31 GPa
480 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 97.2 °C
207 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 103 °C
218 °F
ASTM D1525