Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.05 GPa | 297 ksi | |
Ineos ABS Lustran® Elite HH 1891 Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Europe-Africa-Middle East) Unreinforced PBT+PC alloy. Improved retention of mechanical properties under UV. Excellent low temperature/chemical |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO 527 |
Styrolution Novodur® M210TF ABS Novodur M210TF is medium impact, high gloss injection molding grade designed for toy application. M210TF is in compliance with food contact regulationsInformation provided by Styrolution |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO 527 |
Styrolution PS 576H HIPS Styrolution PS 576H is a high gloss, high impact polystyrene with a good flow and good heat resistance.High gloss HIPSGood flow and heat resistanceHIPS with good balance of mechanical properties and.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Asia Pacific) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Asia Pacific) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO R 527 |
Styron Pulse® A20-95 PC/ABS A medium impact strength PC/ABS blend with high heat distortion and excellent processability.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO 527-2 |
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming This grade belongs to the Total Ecosolution line.Polypropylene PPH 4026 is a polypropylene homopolymer specifically developed to offer outstanding processability for sheet extrusion and thermoformin.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO 527-2 |
Total PSI 4440(EU) High Impact Polystyrene 4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, .. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ASTM D 638 |
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ASTM D 638 |
Cossa Polimeri ESTALUX 9202 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | |
Addcomp PRIEX® 20095 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | |
BASF Polystyrol® 576 H Impact Grade Polystyrene (Europe) Special tough to rigid grade with very good gloss for all types of housings.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | |
Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | blown films MD; ISO 527-3 |
Borealis Bormod™ HC904CF Polypropylene Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL004XXC PC LNP* LUBRICOMP* DL004XXC is a compound based on Polycarbonate containing 20% PTFE. Characteristics of this grade are: Interrnally Lubricated. |