Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | |
Plastcom SLOVALEN PC 93 T 20 PP, 20% mineral filling, UV stabilization FeaturesModified PP for injection moulding with the content of 20 % mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min |
Polimeri Europa KOBLEND HI 41 F1 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Similar to KOBLEND HI 41 with improved fluidity. Main application fields: bumpers Unfilled. Suitable for Injection Molding. Supplied as pellets.ISO data.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | |
Ineos ABS Lustran® Elite HH 1891 Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Asia Pacific) LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Europe-Africa-Middle East) Unreinforced PBT+PC alloy. Improved retention of mechanical properties under UV. Excellent low temperature/chemical |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO 527 |
Styrolution Novodur® M210TF ABS Novodur M210TF is medium impact, high gloss injection molding grade designed for toy application. M210TF is in compliance with food contact regulationsInformation provided by Styrolution |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Asia Pacific) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific) Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Asia Pacific) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO R 527 |
Styron Pulse® A20-95 PC/ABS A medium impact strength PC/ABS blend with high heat distortion and excellent processability.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO 527-2 |
Total PPH 4026 Polypropylene Homopolymer, Film Polypropylene PPH 4026 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min for the cast extrusion of films with outstanding stiffness and heat resistance.Polypropylene PPH 4026 is in.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ASTM D 638 |
Cossa Polimeri ESTALUX 9202 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | |
Addcomp PRIEX® 20095 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | |
Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |