Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 196 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.35 GPa
196 ksi
ISO 527
Quadrant EPP Cesticolor™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Tensile Modulus 1.35 GPa
196 ksi
ISO 527
Quadrant EPP Cestilene™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Tensile Modulus 1.35 GPa
196 ksi
Radici Radilon® A ESL128 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Tensile Modulus 1.35 GPa
196 ksi
1 mm/min
Polimeri Europa EDISTIR PD RR745E High Impact Polystyrene (HIPS)  (discontinued **)
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,088-03-07-12 Environmental stress cracking resistant (ESCR) HIPS. It combines high impact strength with high chemical r..
Tensile Modulus 1.35 GPa
196 ksi
ISO 527
FKuR Kunststoff Terralene® WF 3516 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
Tensile Modulus 1.35 GPa
196 ksi
1 mm/min; ISO 527-1,-2
Inno-Comp INNOPOL® CS 2-4210 10% Chalk-Filled Polypropylene Block-Copolymer
INNOPOL® CS 2-4210 is a 10% chalk-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-4210 is developed for producin..
Tensile Modulus 1.35 GPa
196 ksi
Conditioned; ISO 527-1/-2
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls
PA6, molding grade, micro glass balls, good heat-ageing resistance
Tensile Modulus 1.35 GPa
196 ksi
ISO 527
Iran Petrochemical (PCC) I3S HC 7260(THE) High Density Polyethylene
I3 is a high density polyethylene with 1-Butene as co monomer. It has low warpage, good flowability, high density, hardness and stiffness, good impact strength, and good stress cracking resistance...
Tensile Modulus 1.35 GPa
196 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY M3000 PP
LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat.
Tensile Modulus 1.35 GPa
196 ksi
ISO 527-2
Total PPC 5752 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 5752 is a nucleated controlled-rheology heterophasic copolymer. PPC 5752 is characterized by a high impact resistance and excellent antistatic properties.
Tensile Modulus 1.35 GPa
196 ksi
ISO 527-2
Total PPH 7089 Polypropylene Homopolymer, Fiber
Polypropylene PPH 7089 is a narrow molecular weight distribution homopolymer polypropylene, with anti-gas fading stabilization.Polypropylene PPH 7089 is intended for the extrusion of fibers with the..
Tensile Modulus 1.35 GPa
196 ksi
ISO 527-2
Total PPH 9081 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 9081 is a controlled-rheology homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing improved impact res..
Tensile Modulus 1.35 GPa
196 ksi
ISO 527-2
Total PPH 9082 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 9082 is a controlled-rheology and antistatic homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing impr..
Tensile Modulus 1.35 GPa
196 ksi
ISO 527-2
Total PPM H250 Polypropylene, Homopolymer Medical Grade
Polypropylene PPM H250 is a narrow molecular weight distribution homopolymer with a Melt Flow Index of 25 g/10 min recommended for the manufacture of medical packaging and medical devices, to the ex..
Tensile Modulus 1.35 GPa
196 ksi
ISO 527-2
Total PPC 3640 Polypropylene, Heterophasic Copolymer
ATOFINA Polypropylene PPC 3640 is a nucleated heterophasic copolymer. PPC 3640 is characterized by improved stiffness, creep resistance and high impact resistance.ApplicationPPC 3640 has been devel..
Tensile Modulus 1.35 GPa

@Temperature 23.0 °C
196 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM1300 BK320 TPC-ET  (Unverified Data**)
Hytrel® DYM1300 is a high performance thermoplastic elastomer with high modulus, suited for air bag door applications.Information provided by DuPont Performance Polymers
Tensile Modulus 1.35 GPa
196 ksi
ISO 527-2
Domo 2348TC Polypropylene Copolymer
Information provided by Domo.
Tensile Modulus 1.35 GPa
196 ksi
1 mm/min
Arkema Group Orgalloy® LE 6000IH Nylon Alloy, Flexible Grade (Conditioned)
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).medium viscosity and stiffness, specially suited to the covering of..
Tensile Modulus 1.35 GPa
196 ksi
1 mm/min
Arkema Group Orgalloy® LE 60SF Flexible Nylon Alloy (Conditioned)
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).lower in viscosity than LE 6000, adapted to Suited to the cast film..
Tensile Modulus 1.35 GPa
196 ksi
BASF Novolen® 2348 TC Polypropylene
Grade with nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF.
Copyright © lookpolymers.com All Rights Reserved