Arkema Group Orgalloy® LE 6000IH Nylon Alloy, Flexible Grade (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon, Flexible Alloy
Manufacturer Arkema
Trade Name Orgalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Orgalloy® LE 6000IH Nylon Alloy, Flexible Grade (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).medium viscosity and stiffness, specially suited to the covering of cable and tube. Also suited to injection molding. Flame retardant grade.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
Water Absorption 6.4 %
6.4 %
Moisture Absorption at Equilibrium 1.8 %
1.8 %
Humidity Absorption
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 235 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 4.9 %
4.9 %
50 mm/min
Tensile Modulus 1.35 GPa
196 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min
Vicat Softening Point 97.0 °C
207 °F
50°C/hr; 50N
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V