DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
Manufacturer DuPont Performance Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ISO 527-1/-2
Elongation at Break 1.9 %
1.9 %
ISO 527-1/-2
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527-1/-2
Flexural Strength 200 MPa
29000 psi
ISO 178
Flexural Modulus 10.5 GPa
1520 ksi
ISO 178
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179/1eU
3.00 J/cm²

@Temperature -40.0 °C
14.3 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 179/1eA
0.800 J/cm²

@Temperature -40.0 °C
3.81 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 14.0 µm/m-°C
7.78 µin/in-°F
ISO 11359-1/-2
20.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
11.1 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
73.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
40.6 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
Melting Point 252 °C
486 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 243 °C
469 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ISO 75-1/-2
UL RTI, Electrical 155 °C

@Thickness 0.400 mm
311 °F

@Thickness 0.0157 in
UL 746B
155 °C

@Thickness 0.800 mm
311 °F

@Thickness 0.0315 in
UL 746B
155 °C

@Thickness 1.50 mm
311 °F

@Thickness 0.0591 in
UL 746B
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
IEC 60695-11-10
V-0

@Thickness 0.300 mm
V-0

@Thickness 0.0118 in
IEC 60695-11-10
5VA

@Thickness 1.50 mm
5VA

@Thickness 0.0591 in
IEC 60695-11-20
Electrical Properties Metric English Comments
Comparative Tracking Index 225 V
225 V
IEC 60112
250 - 400 V
250 - 400 V
UL 746A
Descriptive Properties Value Comments
Part Marking Code >PET-GF30FR<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PET-GF30FR(17)
UL recognition UL