Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.1 MPa | 7990 psi | ASTM D638 |
RedEye On Demand VeroBlue PolyJet™ FC840 for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |
|||
Tensile Strength, Yield | 55.1 MPa | 7990 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO.. |
|||
Tensile Strength, Yield | 55.1 MPa | 7990 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers ABSPC 9802 ABS/PC Molding Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 55.1 MPa | 7990 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers ABSPC 9901 ELG ABS/PC Injection Molding Grade, Very High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 55.1 MPa | 7990 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers DIAMALOY 1012 ABS/PBT Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 55.1 MPa | 7990 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP 808 C2 Polycarbonate Alloy, Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 55.1 MPa | 7990 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP 808 C2 TDS Polycarbonate Alloy, Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |