Polymer Property : Tensile Strength, Yield = 55.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.1 MPa
7990 psi
ASTM D638
RedEye On Demand VeroBlue PolyJet™ FC840 for Rapid Prototyping
Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero..
Tensile Strength, Yield 55.1 MPa
7990 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO..
Tensile Strength, Yield 55.1 MPa
7990 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers ABSPC 9802 ABS/PC Molding Grade, High Impact, High Heat
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 55.1 MPa
7990 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers ABSPC 9901 ELG ABS/PC Injection Molding Grade, Very High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 55.1 MPa
7990 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers DIAMALOY 1012 ABS/PBT Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 55.1 MPa
7990 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers NPP 808 C2 Polycarbonate Alloy, Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 55.1 MPa
7990 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers NPP 808 C2 TDS Polycarbonate Alloy, Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.