Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP 808 C2 Polycarbonate Alloy, Natural

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP 808 C2 Polycarbonate Alloy, Natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.35 %

@Temperature 23.0 °C
0.35 %

@Temperature 73.4 °F
Equilibrium; ASTM D570
0.15 %

@Temperature 23.0 °C,
Time 86400 sec
0.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
12 g/10 min

@Load 3.80 kg,
Temperature 230 °C
12 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
78 g/10 min

@Load 1.20 kg,
Temperature 300 °C
78 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.1 MPa
7990 psi
chs 2.0 in/min; ASTM D638
Tensile Modulus 2.067 GPa
299.8 ksi
chs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm,
Temperature 23.0 °C
NB

@Thickness 0.125 in,
Temperature 73.4 °F
reverse notched; ASTM D256
Gardner Impact >= 36.2 J

@Temperature 23.0 °C
>= 26.7 ft-lb

@Temperature 73.4 °F
ASTM D5420
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 90 %
90 %
ASTM D1003
Users viewing this material also viewed the following: