Diamond Polymers DIAMALOY 1012 ABS/PBT Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY 1012 ABS/PBT Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 3.80 kg,
Temperature 260 °C
10 g/10 min

@Load 8.38 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.1 MPa
7990 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.068 GPa
299.9 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 6.675 J/cm

@Thickness 3.17 mm
12.51 ft-lb/in

@Thickness 0.125 in
ASTM D256