Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 724 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
|
FloMet 17-4 PH Stainless Steel, As Sintered FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Yield | 724 MPa | 105000 psi | Tempered at 1150°F, 4hr |
Latrobe Lescalloy® 15-5 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 15-5 VAC-ARC steel is a precipitation hardening martensitic stainless steel commonly considered to be a compositional modification of 17-4 with minimal delta ferrite. A wide range of mec.. |
|||
Tensile Strength, Yield | >= 724 MPa @Strain 0.200 % |
>= 105000 psi @Strain 0.200 % |
H1150 Condition - 620°C at 4 hr |
Latrobe Lescalloy® 15-5 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 15-5 VAC-ARC steel is a precipitation hardening martensitic stainless steel commonly considered to be a compositional modification of 17-4 with minimal delta ferrite. A wide range of mec.. |
|||
Tensile Strength, Yield | >= 724 MPa @Strain 0.200 %, Thickness <=0.400 mm |
>= 105000 psi @Strain 0.200 %, Thickness <=0.0157 in |
CWSR, 0.016 in. Wall & Below; AMS 4944/4945 |
Haynes Ti-3Al-2.5V Alloy Titanium Tubing Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani.. |
|||
Tensile Strength, Yield | >= 724 MPa @Strain 0.200 %, Thickness >=0.400 mm |
>= 105000 psi @Strain 0.200 %, Thickness >=0.0157 in |
CWSR, Above 0.016 in. Wall; AMS 4944/4945 |
Haynes Ti-3Al-2.5V Alloy Titanium Tubing Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani.. |
|||
Tensile Strength, Yield | >= 724 MPa @Strain 0.200 % |
>= 105000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 50 Austenitic Stainless, Level 2 Cold Worked Cold Worked applies to tensile values and are for 0.25 to 4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resis.. |
|||
Tensile Strength, Yield | 724 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
|
Schmolz + Bickenbach MoldMAX® V Copper Alloy Description: Brush Wellman’s MoldMAX® V (MMV) is a high conductivity, moderately high strength, copper nickel silicon chromium alloy. Applications include injection mold and blow mold cores .. |
|||
Tensile Strength, Yield | >= 724 MPa | >= 105000 psi | |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) CWSR Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to CWSR condition; other specific condition entries are also available in MatWeb.Features: Cold formable and w.. |
|||
Tensile Strength, Yield | 724 - 800 MPa | 105000 - 116000 psi | 0.2% offset |
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Spring Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Yield | 724 MPa | 105000 psi | Proportional Limit |
ECOMold 95 Copper Mold Material ECOMold® copper alloys (beryllium-free) are designed specifically for plastics industry applications. ECOMold® 95 has a superior combination of thermal conductivity, hardness, and tensile strengt.. |
|||
Tensile Strength, Yield | 724 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
Tension |
Crucible Steel Aquamet® 17 Martensitic Steel AQUAMET 17 is a precipitation-hardening, martensitic stainless steel. Because it is hardened by a heat treatment, it provides high strength regardless of the diameter. It also offers good toughness .. |
|||
Tensile Strength, Yield | 724 MPa | 105000 psi | |
CMW® THERMKON® 68 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Tensile Strength, Yield | 724 MPa | 105000 psi | Hard |
California Fine Wire Nickel A 200 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 724 MPa @Strain 0.200 %, Temperature -253 °C |
105000 psi @Strain 0.200 %, Temperature -423 °F |
Longitudinal |
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | >= 724 MPa @Strain 0.200 % |
>= 105000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 2 Cold Worked Level 2 Cold Worked applies to tensile and hardness properties of 0.25 to 4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic all.. |
|||
Tensile Strength, Yield | >= 724 MPa @Strain 0.200 % |
>= 105000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 CX105 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |
|||
Tensile Strength, Yield | 724 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
|
Schmolz + Bickenbach MoldMAX XL® Copper Alloy Description: Brush Wellman’s MoldMAX XL® is a high strength copper mold alloy with good thermal conductivity. The alloy contains no beryllium and is available in sections as large as 12” thick. .. |