Schmolz + Bickenbach MoldMAX® V Copper Alloy

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Schmolz + Bickenbach (Swiss Steel International)
Trade Name MoldMAX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schmolz + Bickenbach MoldMAX® V Copper Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Brush Wellman’s MoldMAX® V (MMV) is a high conductivity, moderately high strength, copper nickel silicon chromium alloy. Applications include injection mold and blow mold cores and cavities.Information provided by Schmolz + Bickenbach
Physical Properties Metric English Comments
Density 8.69 g/cc
0.314 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 28
28
Tensile Strength, Ultimate 862 MPa
125000 psi
Tensile Strength, Yield 724 MPa

@Strain 0.200 %
105000 psi

@Strain 0.200 %
Elongation at Yield 7.0 %
7.0 %
Modulus of Elasticity 128 GPa
18500 ksi
Fatigue Strength >= 275 MPa

@# of Cycles 1.00e+7
>= 39900 psi

@# of Cycles 1.00e+7
(R=-1)
Charpy Impact 6.78 J
5.00 ft-lb
Notched
Thermal Properties Metric English Comments
CTE, linear 17.5 µm/m-°C
9.72 µin/in-°F
Specific Heat Capacity 0.410 J/g-°C

@Temperature 100 °C
0.0980 BTU/lb-°F

@Temperature 212 °F
Thermal Conductivity 13.3 W/m-K

@Temperature 100 °C
92.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Melting Point >= 982 °C
>= 1800 °F
approximate
Solidus 982 °C
1800 °F
approximate
Component Elements Properties Metric English Comments
Copper, Cu 88.8 - 91.4 %
88.8 - 91.4 %
Nickel, Ni 6.5 - 7.5 %
6.5 - 7.5 %
Silicon, Si 1.5 - 2.5 %
1.5 - 2.5 %