Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 620 - 800 MPa | 89900 - 116000 psi | |
Materion Beryllium Copper Alloy 25 Strip; H (TD04) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1Formability Ratio (bad Way): 2.9Superficial Hardness: 30T 79-83Tabulated properties appl.. |
|||
Tensile Strength, Yield | 650 - 800 MPa | 94300 - 116000 psi | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM02 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 724 - 800 MPa | 105000 - 116000 psi | 0.2% offset |
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Spring Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |