Polymer Property : Tensile Strength, Yield = 65300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 275 - 450 MPa

@Strain 0.200 %
39900 - 65300 psi

@Strain 0.200 %
Kobe Steel KS60 Commercially Pure Titanium, ASTM Gr. 2, Annealed
Nominal Composition: Ti-Fe-OApplications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Relatively high strength, excellent corrosion resistance..
Tensile Strength, Yield 275 - 450 MPa
39900 - 65300 psi
0.2% proof
Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed
Nominal Composition: Ti-0.4 Ni-0.015 Pd-0.025 Ru-0.14 Cr Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant...
Tensile Strength, Yield 215 - 450 MPa
31200 - 65300 psi
0.2% proof
Kobe Steel KSTI-1.5AL Alpha Titanium Alloy, Annealed
Nominal Composition: Ti-1.5 Al Applications: Exhaust systems.Features:Heat resistant. Information provided by Kobe Steel
Tensile Strength, Yield 275 - 450 MPa
39900 - 65300 psi
0.2% proof
Kobe Steel Titanium alloy with low alloying elements, ASTM Gr. 7, Annealed
Nominal Composition: Ti-0.15 Pd Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by ..
Tensile Strength, Yield 240 - 450 MPa
34800 - 65300 psi
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Tensile Strength, Yield 380 - 450 MPa

@Strain 0.200 %
55100 - 65300 psi

@Strain 0.200 %
SSAB Tunnplat Aluzink 380A YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is ..
Tensile Strength, Yield 280 - 450 MPa

@Strain 0.200 %
40600 - 65300 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 600DL High-strength Steel
High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact..
Tensile Strength, Yield 390 - 450 MPa

@Strain 0.200 %
56600 - 65300 psi

@Strain 0.200 %
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
L direction
ArcelorMittal Save 20-13 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
T direction
ArcelorMittal Save 20-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
L direction
ArcelorMittal Save 25-14 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
T direction
ArcelorMittal Save 25-16 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
L direction
ArcelorMittal Save 27-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
T direction
ArcelorMittal Save 27-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
L direction
ArcelorMittal Save 30-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
T direction
ArcelorMittal Save 30-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 380 - 450 MPa
55100 - 65300 psi
ArcelorMittal HSLA 380 High strength low alloy steel for cold forming, Cold Rolled
Available in the following: uncoated (HC380LA), electroglavanized (HC380LA +ZE) and Extragal®/galfan/Galvannealed (HC380LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range ..