Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 215 - 450 MPa | 31200 - 65300 psi | 0.2% proof |
Kobe Steel KSTI-1.5AL Alpha Titanium Alloy, Annealed Nominal Composition: Ti-1.5 Al Applications: Exhaust systems.Features:Heat resistant. Information provided by Kobe Steel |
|||
Tensile Strength, Yield | 215 MPa @Strain 0.200 %, Temperature 980 °C |
31200 psi @Strain 0.200 %, Temperature 1800 °F |
|
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 215 MPa @Temperature 870 °C |
31200 psi @Temperature 1600 °F |
|
Haynes Hastelloy® W alloy as a weld filler, base metal Multimet alloy 12.7 mm plate weldment Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Tensile Strength, Yield | 215 MPa @Strain 0.200 %, Temperature 649 °C |
31200 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes HR-160® alloy, solution annealed sheet Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Yield | 215 MPa @Strain 0.200 % |
31200 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals INCOLOY® Alloy DS A nickel-iron-chromium alloy with an addition of silicon. It has good high-temperature strength and excellent resistance to oxidation and carburization. The silicon content makes the alloy resista.. |
|||
Tensile Strength, Yield | 215 MPa | 31200 psi | ASTM D638 |
Solvay TECHNYL® 2912GMH7-P PA66, 63% glass fiber, DRY Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offerin.. |
|||
Tensile Strength, Yield | 215 MPa | 31200 psi | ISO 527 |
Polyram PlusTek RA303G50 Nylon 66 for Injection Molding, 50% Glass Fiber Reinforced, Heat Stabilized, Hydrolysis Resistant 50% Glass fiber reinforced, heat stabilized and hydrolysis resistant Nylon 66 for injection molding applications.Information provided by Polyram. |