Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 275 - 450 MPa @Strain 0.200 % |
39900 - 65300 psi @Strain 0.200 % |
|
Kobe Steel KS60 Commercially Pure Titanium, ASTM Gr. 2, Annealed Nominal Composition: Ti-Fe-OApplications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Relatively high strength, excellent corrosion resistance.. |
|||
Tensile Strength, Yield | 275 - 450 MPa | 39900 - 65300 psi | 0.2% proof |
Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed Nominal Composition: Ti-0.4 Ni-0.015 Pd-0.025 Ru-0.14 Cr Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant... |
|||
Tensile Strength, Yield | 215 - 450 MPa | 31200 - 65300 psi | 0.2% proof |
Kobe Steel KSTI-1.5AL Alpha Titanium Alloy, Annealed Nominal Composition: Ti-1.5 Al Applications: Exhaust systems.Features:Heat resistant. Information provided by Kobe Steel |
|||
Tensile Strength, Yield | 275 - 450 MPa | 39900 - 65300 psi | 0.2% proof |
Kobe Steel Titanium alloy with low alloying elements, ASTM Gr. 7, Annealed Nominal Composition: Ti-0.15 Pd Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by .. |
|||
Tensile Strength, Yield | 240 - 450 MPa | 34800 - 65300 psi | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Yield | 380 - 450 MPa @Strain 0.200 % |
55100 - 65300 psi @Strain 0.200 % |
|
SSAB Tunnplat Aluzink 380A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Tensile Strength, Yield | 280 - 450 MPa @Strain 0.200 % |
40600 - 65300 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 600DL High-strength Steel High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact.. |
|||
Tensile Strength, Yield | 390 - 450 MPa @Strain 0.200 % |
56600 - 65300 psi @Strain 0.200 % |
|
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | L direction |
ArcelorMittal Save 20-13 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | T direction |
ArcelorMittal Save 20-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | L direction |
ArcelorMittal Save 25-14 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | T direction |
ArcelorMittal Save 25-16 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | L direction |
ArcelorMittal Save 27-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | T direction |
ArcelorMittal Save 27-17 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | L direction |
ArcelorMittal Save 30-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | T direction |
ArcelorMittal Save 30-17 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 380 - 450 MPa | 55100 - 65300 psi | |
ArcelorMittal HSLA 380 High strength low alloy steel for cold forming, Cold Rolled Available in the following: uncoated (HC380LA), electroglavanized (HC380LA +ZE) and Extragal®/galfan/Galvannealed (HC380LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range .. |