Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 390 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 390 MPa

@Strain 0.200 %
56600 psi

@Strain 0.200 %
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield 390 MPa

@Temperature 760 °C
56600 psi

@Temperature 1400 °F
Haynes Hastelloy® W alloy, shielded metal arc welds, aged 1000 hours at 650°C (1200°F)
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Yield 390 MPa

@Strain 0.200 %
56500 psi

@Strain 0.200 %
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C) + Aged 1400°F (760°C)
Tensile strength (ultimate and yield), elongation, and hardness values are for samples annealed 2150°F (1180°C)/5 minutes/AC + Aged 1400°F (760°C)/100h/AC. This produces ASTM grain siz..
Tensile Strength, Yield 390 - 540 MPa

@Strain 0.200 %
56600 - 78300 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 800 DL High-strength Steel
In course of development.Data provided by SSAB Tunnplat.
Tensile Strength, Yield >= 390 MPa
>= 56600 psi
SSAB Tunnplat Domex® 390XP Extra High-strength Cold-forming Steel
Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene..
Tensile Strength, Yield >= 390 MPa
>= 56600 psi
SSAB Tunnplat Domex® 390YP Cold-forming Steel, HSLA
Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®..
Tensile Strength, Yield 390 - 450 MPa

@Strain 0.200 %
56600 - 65300 psi

@Strain 0.200 %
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Tensile Strength, Yield 390 - 430 MPa
56600 - 62400 psi
L direction
ArcelorMittal Save 20-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 390 - 430 MPa
56600 - 62400 psi
L direction
ArcelorMittal Save 25-16 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 390 - 430 MPa
56600 - 62400 psi
L direction
ArcelorMittal Save 27-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 390 - 430 MPa
56600 - 62400 psi
L direction
ArcelorMittal Save 30-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 390 MPa

@Strain 0.200 %
56600 psi

@Strain 0.200 %
Haynes 230® alloy, cold rolled and 1232°C solution annealed sheet
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Copyright © lookpolymers.com All Rights Reserved