Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 390 MPa @Strain 0.200 % |
56600 psi @Strain 0.200 % |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | 390 MPa @Temperature 760 °C |
56600 psi @Temperature 1400 °F |
|
Haynes Hastelloy® W alloy, shielded metal arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Tensile Strength, Yield | 390 - 540 MPa @Strain 0.200 % |
56600 - 78300 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 800 DL High-strength Steel In course of development.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Yield | >= 390 MPa | >= 56600 psi | |
SSAB Tunnplat Domex® 390XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Tensile Strength, Yield | >= 390 MPa | >= 56600 psi | |
SSAB Tunnplat Domex® 390YP Cold-forming Steel, HSLA Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®.. |
|||
Tensile Strength, Yield | 390 - 450 MPa @Strain 0.200 % |
56600 - 65300 psi @Strain 0.200 % |
|
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Tensile Strength, Yield | 390 - 430 MPa | 56600 - 62400 psi | L direction |
ArcelorMittal Save 20-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 390 - 430 MPa | 56600 - 62400 psi | L direction |
ArcelorMittal Save 25-16 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 390 - 430 MPa | 56600 - 62400 psi | L direction |
ArcelorMittal Save 27-17 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 390 - 430 MPa | 56600 - 62400 psi | L direction |
ArcelorMittal Save 30-17 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 390 MPa @Strain 0.200 % |
56600 psi @Strain 0.200 % |
|
Haynes 230® alloy, cold rolled and 1232°C solution annealed sheet Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |