ThyssenKrupp 12Ni5 Structural Steel

Category Metal , Ferrous Metal
Manufacturer ThyssenKrupp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ThyssenKrupp 12Ni5 Structural Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
5% nickel steel for low temperature service down to -165°FApplication for pressure vessels and tanks for the transportation and storage of ethyleneReference: 5.000 t/y in thicknesses up to 2 in.Heat treatment: quenched and temperedInformation Provided by Thyssen Krupp
Mechanical Properties Metric English Comments
Tensile Strength at Break 552 - 758 MPa
80100 - 110000 psi
Tensile Strength, Yield >= 414 MPa
>= 60000 psi