Niagara LaSalle 1213 Cold Finished Steel Bar

Category Metal , Ferrous Metal , Carbon Steel , AISI 1000 Series Steel
Manufacturer Niagara LaSalle
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niagara LaSalle 1213 Cold Finished Steel Bar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The A.I.S.I. grade 1215 has essentially eliminated a number of similar free machining grades, such as 1212. Both 1215 and 1213 machine considerably faster than 1212 and provide good surface finish and brazing properties. These steels are difficult to weld and are not recommended for case hardening. They are generally used where mechanical properties can be sacrificed for machinabilityInformation provided by Niagra LaSalle Corporation
Mechanical Properties Metric English Comments
Hardness, Brinell 167
167
Tensile Strength 538 MPa
78000 psi
Tensile Strength, Yield 414 MPa
60000 psi
Elongation at Break >= 10 %
>= 10 %
2"
Reduction of Area 35 %
35 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.13 %
<= 0.13 %
Iron, Fe 98.42 - 98.99 %
98.42 - 98.99 %
as balance
Manganese, Mn 0.70 - 1.0 %
0.70 - 1.0 %
Phosphorous, P 0.070 - 0.12 %
0.070 - 0.12 %
Sulfur, S 0.24 - 0.33 %
0.24 - 0.33 %