Universal Wire Works ER90SB-9 Steel Welding Wire

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works ER90SB-9 Steel Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal 90S-B9 is used primarily for welding the higher chromium alloyed 9CrMoNbV steels A213 (T-91), A335 (p-91), A387 (Gr-91) used where elevated temperatures and pressures are required. The advantages of this alloy are improved toughness and better creep properties, which ultimately allow for higher steam temperatures and the use of thinner piping materials. Due to the higher elevated temperature properties of this alloy, components that are now fabricated from stainless and ferritic steels may be fabricated from a single alloy, eliminating problems that are associated with dissimilar welds.Preheat/Interpass Temp. 300/500°FInformation provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 621 MPa
90000 psi
AR-5% O2
Tensile Strength, Yield 414 MPa
60000 psi
AR-5% O2
Elongation at Break 16 %
16 %
Component Elements Properties Metric English Comments
Carbon, C 0.070 - 0.13 %
0.070 - 0.13 %
Chromium, Cr 8.0 - 9.5 %
8.0 - 9.5 %
Copper, Cu 0.20 %
0.20 %
Iron, Fe 86.1 - 88.3 %
86.1 - 88.3 %
As Remainder
Manganese, Mn 1.25 %
1.25 %
Molybdenum, Mo 0.80 - 1.1 %
0.80 - 1.1 %
Nickel, Ni 1.0 %
1.0 %
Niobium, Nb (Columbium, Cb) 0.020 - 0.10 %
0.020 - 0.10 %
Nitrogen, N 0.030 - 0.070 %
0.030 - 0.070 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.15 - 0.30 %
0.15 - 0.30 %
Sulfur, S 0.010 %
0.010 %
Vanadium, V 0.15 - 0.25 %
0.15 - 0.25 %