Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.21 MPa
900 psi
TM R050-36
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11..
Tensile Strength, Yield 6.21 MPa
900 psi
TM R050-36
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP1112NC Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Black is a modified version of the standard EP11..
Tensile Strength, Yield 6.21 MPa

@Strain 300 %
901 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Synprene® RT-3880M Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D638
Multibase Multi-Flex® D 4210 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, GoodStiffness, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation p..
Tensile Strength, Yield 6.21 MPa
900 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 7025 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Tensile Strength, Yield 6.21 MPa
900 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 7130 Fluorocarbon-Elastomer
FKM specially for oil & gas service.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 6.21 MPa
900 psi
Tensile strength decreases by 10% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Saint-Gobain COHRlastic® 9040 Wide Series General Purpose Silicone Solid Rubber
Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome..
Tensile Strength, Yield 6.21 MPa
900 psi
100%; ASTM D412
Teknor Apex APEX® 3211-75 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Tensile Strength, Yield 6.21 MPa
900 psi
100%; ASTM D412
Teknor Apex APEX® 3300-75 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex Flexalloy® 9100-35 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex MONPRENE® MP 2830M Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex MONPRENE® MP 2835E Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 6.21 MPa
900 psi
Tensile strength decreases by 10% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Saint-Gobain COHRlastic® 9050 Wide Series General Purpose Silicone Solid Rubber
Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome..
Tensile Strength, Yield 6.21 MPa
900 psi
100%; ASTM D412
Teknor Apex APEX® 3200-75 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex TEKBOND® 6000-35 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex TEKBOND® 6000-75 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex TEKRON® 4000-40 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 6.21 MPa
900 psi
at 200%; ASTM D412
Lubrizol Estane® ALR E80A Thermoplastic Polyurethane
Type: Estane® ALR E80A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Information Provided by The Lubrizol Corporation
Tensile Strength, Yield 6.21 MPa
900 psi
at 300%; ASTM D412
Lubrizol Estane® MVT 75AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 75AT3 is a 75A aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and..
Tensile Strength, Yield 6.21 MPa
900 psi
at 100%; ASTM D412
Lubrizol Estane® MVT 90AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 90AF3 TPU is a 90A aromatic polyether-based thermoplastic polyurethane.Features: High moisture vapor transmission, good physical properties and elasticity, free of organo-tin comp..
Tensile Strength, Yield 6.21 MPa

@Temperature 21.1 °C
900 psi

@Temperature 70.0 °F
Flatwise Tensile; 15 Cycles, Thermal Cycling
Hexcel® Redux® HP655 Toughened BMI film Adhesive
Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655..
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D638
Clariant Renol PUR1100SS15 Polyurethane Elastomer, Stainless Fiber, EMI/RFI/ESD
Data provided by Clariant Masterbatches
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex Monprene® MP-2835E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength, Yield 6.21 MPa
900 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® IT 36-021 NATURAL Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Specialty Thermoplastic ElastomerApplications: FDA (Food Contact)Processing Method: Injection MoldingInformation provided by PolyOne Corporation
Tensile Strength, Yield 6.21 MPa
900 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3945 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti..
Tensile Strength, Yield 6.21 MPa
900 psi
TM R050-36
Resinlab® EP1026R Rubber Modified Epoxy Adhesive
Resinlab™ EP1026R is a two part unfilled rubber modified epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free ..
Copyright © lookpolymers.com All Rights Reserved