Lubrizol Estane® MVT 75AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® MVT 75AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Type: Estane® MVT 75AT3 is a 75A aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and elasticity.Uses: Blown and flat die/cast film extrusion, injection molding and cable jacketing.Information Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 78

@Time 5.00 sec
72 - 78

@Time 0.00139 hour
ASTM D2240
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D412
Tensile Strength, Yield 4.14 MPa
600 psi
at 100%; ASTM D412
6.21 MPa
900 psi
at 300%; ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
Tear Strength 19.3 kN/m
110 pli
Trouser; ASTM D470
Graves Tear Strength 63.1 kN/m
360 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 20

@Load 1.00 kg
20

@Load 2.20 lb
H-18 wheel; ASTM D3389
Thermal Properties Metric English Comments
Melting Point 136 °C
277 °F
DSC
Glass Transition Temp, Tg -68.0 °C
-90.4 °F
DSC