Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D792
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Electrical Properties Metric English Comments
Surface Resistivity per Square 10000 ohm - 1e+05
10000 ohm - 1e+05
ASTM D257
Processing Properties Metric English Comments
Dry Time 2 - 4 hour

@Temperature 104 °C
2 - 4 hour

@Temperature 220 °F
to ensure moisture level is less than 0.02%